Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 14.4 MPa | 2090 psi | Aluminum-Stainless; Tensile Lap Shear |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |