Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 1644 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 11.33 MPa
1644 psi
Lap Shear; ASTM D1002
DuPont™ Fusabond® E158 Polymer Modifier
DuPont™ Fusabond® E158 is a anhydride modified polyethylene. Uses: Adhesives Pipe Coating Tie-Layer
Adhesive Bond Strength 11.33 MPa
1644 psi
Lap Shear; ASTM D1002
DuPont™ Fusabond® E158H Polymer Modifier
DuPont™ Fusabond® E158H is a anhydride modified polyethylene. Uses: Adhesives Coating Applications Pipe Coating Tie-Layer
Copyright © lookpolymers.com All Rights Reserved