Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 19.7 MPa | 2850 psi | Lap shear, alum to alum, 24 hrs @ 25°C |
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit.. |
|||
Adhesive Bond Strength | 19.7 MPa @Temperature 25.0 °C |
2850 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-1/V Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |