Polymer Property : Adhesive Bond Strength = 2.04 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 2.04 MPa
296 psi
"Wet" Lap Shear Strength (49.0 MPa Hemming Press.)
Dow BETAMATE™ 73345G Epoxy
BETAMATE™ 73345G is a one-part, high performance, heat curing, epoxy adhesive. It is capable of bonding oily galvanized and cold rolled steel without a primer and has corrosion resistance. BETAMA..