Adhesive Bond Strength 2.41 - 2.76 MPa
350 - 400 psi
Sika Industry SikaFlex 252 One Part Polyurethane Adhesive
Sika 252 SikaFlex One Part Polyurethane AdhesiveA high viscous, high strength adhesive, this product can replace rivets, screws, welds, and other mechanical fasteners. Seals and bonds in one step. 4..
Adhesive Bond Strength 2.41 MPa
350 psi
Lap shear, alum to alum, @ 25°C
Tra-Con Tra-Bond 872-7TN1 Flexible Thixotropic Epoxy Adhesive
TRA-BOND 872-7TN1 is a flexible thixotropic epoxy. The high viscosity and long worklife make this material easy to handle. Also, the high thermal conductivity makes this product ideal for electronic..