Adhesive Bond Strength 160 MPa

@Diameter <=100 mm
23200 psi

@Diameter <=3.94 in
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
Elektro-Isola Etronit B 65 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: For mechanical and electrical low-voltage applications. Good electrical properties at normal air humidity.Applications: Winding tubes in the foil and metal foil industries and carrier t..
Adhesive Bond Strength 160 MPa

@Diameter <=100 mm
23200 psi

@Diameter <=3.94 in
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3
Elektro-Isola Etronit B67 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: For mechanical and electrical low-voltage applications. Very good electrical properties at high air humidity. Applications: Winding tubes in the foil and metal foil industries and carri..