Mechanical Properties Metric English Comments
Adhesive Bond Strength 34.5 MPa
5000 psi
Varies with substrates
Loctite® 3292 Acrylic Bonding Adhesive
Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. ..
Adhesive Bond Strength 34.5 MPa
5000 psi
Lap shear, alum to alum, @ 25°C
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive
TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc..
Adhesive Bond Strength 34.5 MPa
5000 psi
Lap shear, alum to alum
Tra-Con Tra-Bond 970-3 Room Temperature Cure General Purpose Adhesive
TRA-BOND 970-3 general purpose adhesive is a non-flowing blue paste. This adhesive cures at room temperature. This adhesive is available in kits with a mix ratio of 100 parts A to 74 parts B or prem..
Adhesive Bond Strength 34.5 MPa
5000 psi
Steel-Steel; after optimum cure
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio
Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati..
Adhesive Bond Strength 34.5 MPa
5000 psi
Steel-Steel; after optimum cure
Armstrong C-7/W Epoxy Adhesive, 2:3 Mix Ratio
A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may ..