Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 26.79 MPa | 3885 psi | |
Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 85 Metal Bonder Fusion™ Cyanoacrylate Instant Ethyl Adhesive |