Mechanical Properties Metric English Comments
Adhesive Bond Strength 4.13 MPa
599 psi
PVC, Substrate Failure, Shear; ASTM D1002
Permabond 932 Cyanoacrylate
PERMABOND 932 is a low odor, non­fogging, non­frosting cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesiv..