Mechanical Properties Metric English Comments
Adhesive Bond Strength 0.0302 MPa

@Thickness 25.4 mm
4.38 psi

@Thickness 1.00 in
Aremco Pyro-Tape™ 682-AR High Temperature Tape Single-layer ultra-high molecular weight polyethylene with a rubber adhesive
Applications Abrasion Resistance Features Low coefficient of friction to reduce wear, scratching and noise. Liners for chutes, rails and slides.