Mechanical Properties Metric English Comments
Adhesive Bond Strength 3.24 MPa
470 psi
Lap shear, on primed Al
Momentive Performance Materials RTV566 Silicone Rubber Compound for Low Outgassing Applications
RTV566 silicone rubber compound is a two-part product processed and tested for applications where low outgassing is required. RTV566A base compound is supplied ready to use with RTV566B curing agen..