Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 32.8 MPa | 4750 psi | Steel-Steel; after optimum cure |
Armstrong A-10-T Epoxy Adhesive Clear, thixotropic, 5-minute cure general-purpose epoxy adhesive. Provides rapid high strength bonds to many substrates. Supplied in 1:1 ratio dispense kits for easy application.Information provid.. |
|||
Adhesive Bond Strength | 32.8 MPa @Temperature 25.0 °C |
4750 psi @Temperature 77.0 °F |
Aluminum-Aluminum tensile shear |
Armstrong A-12-T Epoxy Adhesive Provides the same basic properties as A-12, but in thixotropic, non-sag, easily-brushable paste form. An ideal material for use where adhesive flow during cure cannot be tolerated. A-12-T meets t.. |