Polymer Property : Adhesive Bond Strength = 5080 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 35.0 MPa
5080 psi
steel collar and pin shear; ISO 10123
Permabond A1046 Anaerobic Retainer
Permabond® A1046 is a rapid curing adhesive designed to provide permanent locking and sealing of metal parts such as bearings, gears, pulleys and threaded components. It exhibits high strength and ..