Mechanical Properties Metric English Comments
Adhesive Bond Strength 20.0 - 35.0 MPa
2900 - 5080 psi
Steel , Shear; ISO 4587
Permabond ES562 Epoxy Resin
PERMABOND® ES562 is a single-part epoxy adhesive which flows like solder when heated during curing. The adhesive has excellent adhesion to metal surfaces and composites. The high bond strength of t..
Adhesive Bond Strength 0.690 - 35.0 MPa
100 - 5080 psi
Average value: 15.7 MPa Grade Count:238
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Adhesive Bond Strength 33.0 - 35.0 MPa
4790 - 5080 psi
Mild steel, Shear
Permabond TA4246 Toughened Acrylic Adhesive
PERMABOND® TA4246 is a 2-part, no-mix, room temperature curing structural adhesive. It is ideal for use on a wide variety of substrate materials and forms a very high strength structural bond with ..