Polymer Property : Adhesive Bond Strength = 5250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 36.2 MPa
5250 psi
Steel-Steel; after optimum cure
Armstrong C-4/W Epoxy Adhesive
A low viscosity, clear amber, unfilled adhesive, recommended for use with activators D or W. C-4 with Activator W offers maximum versatility in that differing degrees of flexibility can be achieved ..