Polymer Property : Adhesive Bond Strength = 5800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 40.0 MPa
5800 psi
Trelleborg Emerson & Cuming Eccobond® G 909 One-Component Fast Cure Epoxy Adhesive
Emerson & Cuming G 909 Eccobond® One-Component Fast Cure Epoxy AdhesiveHigh strength, thixotropic, flexible, epoxy adhesive. High peel strength (30 pli). Recommended for bonding copper, aluminum an..