Mechanical Properties Metric English Comments
Adhesive Bond Strength 59.6 MPa
8650 psi
Steel-Steel; after optimum cure
Armstrong A-3/A Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..
Adhesive Bond Strength 59.6 MPa
8650 psi
Steel-Steel; after optimum cure
Armstrong A-3/E Epoxy Adhesive
A Jet black epoxy paste especially formulated for bonding rigid materials. When used with Activator A or E, A-3 exhibits excellent bonding properties to phenolics, precious stones, ceramics, glass,..