300% Modulus 0.000310 GPa
0.0450 ksi
ASTM D412
Northstar Polymers MPP-V37A Polyurethane Gel Elastomer
This two-component polyurethane casting system makes type of soft elastomer material known as “gel”. Applications for this material include filling component for computer keyboard/mouse-pad wrist..