Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000469 GPa @Time 7200 sec |
0.0680 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7030-1000 TPE Product Description: StarMediflex P 7030-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |
|||
300% Modulus | 0.000469 GPa @Time 7200 sec |
0.0680 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarMediflex P 7035-1000 TPE Product Description: StarMediflex P 7035-1000 is an easy processing TPE designed for injection molding. This particular class of TPE material for medical products and tubing applications. Features:S.. |