Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000490 GPa | 0.0711 ksi | JIS K6301 |
Stellarchem AB835EM-1 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed unconventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, completel.. |
|||
300% Modulus | 0.000490 GPa | 0.0711 ksi | JIS K6301 |
Stellarchem DIOSHY® GP-935-UB2 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000490 GPa | 0.0711 ksi | JIS K6301 |
Stellarchem DIOSHY® MP-960NC TPE Compound This grade of Stellarchem MP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
300% Modulus | 0.000490 GPa | 0.0711 ksi | JIS K6301 |
Stellarchem FP-860 TPE Compound Product description : This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric poly.. |
|||
300% Modulus | 0.000490 GPa | 0.0711 ksi | JIS K6301 |
Stellarchem GP-945 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000490 GPa | 0.0711 ksi | JIS K6301 |
Stellarchem LP-845 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000490 GPa | 0.0711 ksi | JIS K6301 |
Stellarchem MP-850 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |