Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 300% Modulus = 0.00124 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00124 GPa
0.180 ksi
ASTM D 412
CPT C-Flex® R70-005 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
300% Modulus 0.00124 GPa
0.180 ksi
High-K Stress Control Tube; ASTM D412
3M 7620-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
300% Modulus 0.00124 GPa
0.180 ksi
High-K Stress Control Tube; ASTM D412
3M 7680-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
300% Modulus 0.00124 GPa
0.180 ksi
High-K Stress Control Tube; ASTM D412
3M 7690-S Cold Shrink QT-III Silicone Rubber Skirted Termination Kits
3M™ Cold Shrink QT-III Silicone Rubber Skirted Termination Kits, 7620-S, 7680-S and 7690-S Series, contain one-piece, skirted, silicone Rubber Skirted Terminations, qualified as IEEE Standard 48 Cl..
Copyright © lookpolymers.com All Rights Reserved