Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00152 GPa | 0.220 ksi | ASTM D 412 |
CPT C-Flex® R70-028 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
300% Modulus | 0.00152 GPa | 0.220 ksi | ASTM D 412 |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
300% Modulus | 0.00152 GPa | 0.220 ksi | ASTM D 412 |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |