Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00169 GPa @Time 7200 sec |
0.245 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-9 TPE Product Description: StarTUFF TF 45-LR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |