Polymer Property : 300% Modulus = 0.00186 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00186 GPa
0.270 ksi
Typical properties of film cast form toluene solution; ASTM D412
Kraton® D1114 P (SIS) Linear Triblock Copolymer
Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: ..
300% Modulus 0.00186 GPa

@Time 7200 sec
0.270 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 65-HR-9 TPE
Product Description: StarTUFF TF 65-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M..