Mechanical Properties Metric English Comments
300% Modulus 0.00209 GPa
0.303 ksi
ASTM D412
Kraton® G7720 GI-N (SEBS) Compound
Description: Kraton G7720 GI-N is an easy processing, general purpose 57 Shore a hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..