Mechanical Properties Metric English Comments
300% Modulus 0.00414 GPa
0.600 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00414 GPa
0.600 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00414 GPa
0.600 ksi
AdvanSource Biomaterials ChronoFlex® AL 80A Biodurable Medical Grade Polyurethane
ChronoFlex® AL is a family of premium polycarbonate aliphatic biodurable thermoplastic polyurethane elastomers developed by AdvanSource Biomaterials Corporation. ChronoFlex® AL medical-grade elas..
300% Modulus 0.00414 GPa
0.600 ksi
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® IT 38-034 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Extrusion and MoldingPolyOne First ChoiceDisclaimer: A..