Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.005516 GPa | 0.8000 ksi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® 12C75 Thermoplastic Polyurethane Elastomer Pearlthane® 12C75 is a standard polyester based TPU supplied in form of translucent, colorless pellets, specially designed for compounds in which TPU is used as an additive. Features include low .. |