Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00610 GPa | 0.885 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00610 GPa | 0.885 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00610 GPa | 0.885 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00610 GPa | 0.885 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR Polyfil HG90 Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00610 GPa | 0.885 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR N990 (MT) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
300% Modulus | 0.00610 GPa | 0.885 ksi | |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Talc-Mistron Vapor MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |