Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.007894 GPa | 1.145 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-990 (MT) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.007894 GPa | 1.145 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TP-95 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.007894 GPa | 1.145 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 40 PHR Carbon Black, N-990 (MT) Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
300% Modulus | 0.007894 GPa | 1.145 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with TP-95 Plasticizer MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |