Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 310ºF Cure Temperature MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 90 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 83A MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 310ºF Cure Temperature MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 120 PHR N990 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00896 GPa | 1.30 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N339 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |