Mechanical Properties Metric English Comments
300% Modulus 0.008998 GPa
1.305 ksi
ASTM D412
Lubrizol Advanced Materials PEARLTHANE® 12K85LB Thermoplastic Polyurethane Elastomer  (discontinued **)
PEARLTHANE® 12K85 LB is a standard polyester-based TPU with a lubricating additive, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mech..
300% Modulus 0.008998 GPa
1.305 ksi
ISO 527-2/5A/500
Lubrizol Advanced Materials PEARLTHANE® 91T85 Thermoplastic Polyurethane Elastomer
Type : Pearlthane® 91T85 is a aliphatic-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Low density, fast processing and excellent elasticity properties.A..