Mechanical Properties Metric English Comments
300% Modulus 0.0118 GPa
1.71 ksi
Cured
KKPC Kumho KHS 68 High Styrene Resin Masterbatch (HSR)
High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve..
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPU-B95 General Grade, Blow Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Blow MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPU-BH95 Hydrolysis Resistance, Blow Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPU-C95 General Grade, Calender Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPU-CH95 High Hydrolysis Resistance, Calender Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPUI-E90 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan PU Corporation TPUI-L85 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan Sheen Soon Sheenthane® A8550 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan Sheen Soon Sheenthane® A8630F Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0118 GPa
1.71 ksi
Taiwan Sheen Soon Sheenthane® A9200B Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionHalogen-free fire-retardant gradeInformation provided by Taiwan Sheen Soon Co., LTD.