Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.01207 GPa
1.751 ksi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® G7723 G Linear Triblock Copolymer
Description: Kraton G7723 GS-N is a linear triblock copolymer based on styrene and ethylene/butylene. It is supplied from North America in the physical form identified: G4610 HU - supplied as an und..