Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0152 GPa | 2.20 ksi | |
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-85A elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced UV stability and good hydrolytic stab.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0152 GPa | 2.21 ksi | ASTM D412 |
Huntsman IROGRAN® PS 440-200 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | 150°C, 40 min., Pressure Vulcanization. 21% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 25M Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | 150°C, 40 min., Pressure Vulcanization. 47% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 40H Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
SK Chemicals SKYTHANE® X585A Polyester Based Thermoplastic Polyurethane Elastomer Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
Styron Sprintan® SLR 4602 Solution Styrene Butadiene Rubber (S-SBR) Composition: SPRINTAN® SLR-4602 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure a.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | |
Elastomer Engineering E900-90A Polyurethane A polyether-based urethane that is excellent in water treatment applications. Typical uses: Wheels, casters, rolls, metal forming strippers and pads. Information provided by Elastomer Engineering I.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.50 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 1.5 PHR Sulfur MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
Lubrizol Estane® ALR PC85A Thermoplastic Polyurethane Type: Estane® ALR PC85A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | ASTM D412 |
Lubrizol Estane® 2355-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Damping capacityAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009... |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 0.50 PHR Caytur 4 MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 1.5 PHR Sulfur MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0152 GPa | 2.20 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 60 PHR N774 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |