Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0162 GPa | 2.35 ksi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.0162 GPa | 2.35 ksi | Vulcanized |
KKPC KOSYN 1507L Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
300% Modulus | 0.0162 GPa | 2.35 ksi | 150°C, 40 min., Pressure Vulcanization. 24% Change after 100°C, 70 hrs, Oil Immersion |
KKPC KOSYN KNB 25LH Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
300% Modulus | 0.0162 GPa | 2.35 ksi | aged in air at 100ºC for 4 days |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with Monoplex DOS Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |