Mechanical Properties Metric English Comments
300% Modulus 0.0182 GPa
2.64 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0182 GPa
2.64 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 70A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0182 GPa
2.64 ksi
DIN 53504
Lubrizol ESTANE® 58360 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..