Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0226 GPa | 3.27 ksi | Cured |
KKPC Kumho RM 21 High Styrene Resin Masterbatch (HSR) High Styrene Resin Masterbatch (HSR)Characteristics: KOSYN KHS is produced by mixing SBR 1502 of 23.5% styrene and high styrene resin latex at high temperature. It works as plasticizer which improve.. |
|||
300% Modulus | 0.0226 GPa | 3.27 ksi | |
Taiwan Sheen Soon Sheenthane® A9610 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |