Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.02748 GPa
3.985 ksi
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..
300% Modulus 0.02748 GPa
3.985 ksi
Formulation Example
TSE Industries Millathane® 66 Millable Polyurethane Rubber
Millathane 66 is a peroxide-curable polyurethane rubber for the production of oil, fuel and chemical resistant parts which require excellent low and high temperature performance and high mechanical ..