Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0374 GPa | 5.42 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR2202-95A Seal Grade TPU Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |