Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.000981 GPa | 0.142 ksi | JIS K6301 |
Stellarchem GP-860HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
300% Modulus | 0.000981 GPa | 0.142 ksi | JIS K6301 |
Stellarchem GP-965B TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |