Polymer Property : 300% Modulus = 0.189 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00130 GPa
0.189 ksi
ASTM D412
Polimeri Europa Europrene® SOL T 9113 Styrene - Isoprene Block Copolymer
Europrene® SOL T 9113 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 18% weight and diblock content is..
300% Modulus 0.00130 GPa
0.189 ksi
ASTM D 638
API Megol AM DP2375/30 SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..