Polymer Property : 300% Modulus = 0.280 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00193 GPa

@Time 7200 sec
0.280 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarGrip GP 55-1000 TPE
Product Description: StarGrip GP 55-1000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery..
300% Modulus 0.00193 GPa

@Time 7200 sec
0.280 ksi

@Time 2.00 hour
Die C; ASTM D412
STAR Thermoplastic Alloys & Rubbers StarGrip GP 55-9000 TPE
Product Description: StarGrip GP 55-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery..
300% Modulus 0.00193 GPa
0.280 ksi
ASTM D 412
CPT C-Flex® R70-001 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..