300% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
300% Modulus 0.00310 GPa
0.450 ksi
Kuraray SEPTON® S64 Soft Compound
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its unique isoprene technology. SEPTON® resins are a series of hydrogenated styre..
300% Modulus 0.00310 GPa
0.450 ksi
ASTM D412
Teknor Apex MONPRENE® MP 2870E Thermoplastic Elastomer
Information provided by Teknor Apex Company
300% Modulus 0.00310 GPa
0.450 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 10 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..