Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00470 GPa | 0.682 ksi | |
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 61 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
300% Modulus | 0.00470 GPa | 0.682 ksi | |
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 58 Shore A
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60.. |
|||
300% Modulus | 0.00470 GPa | 0.682 ksi | ASTM D412; ASTM D638 |
Lubrizol Estane® 58252 Thermoplastic Polyurethane Type: Estane® 58252 is a 70A polyether-type thermoplastic polyurethane (TPU).Features: Formulated to have one of the highest MVT values within the thermoplastic polyurethane class. It is also amon.. |