Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00560 GPa
0.812 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
300% Modulus 0.00560 GPa
0.812 ksi
Measured on films cast from a solution in toluene; ASTM D412
Kraton® G1650 E (SEBS) Linear Block Copolymer
Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i..
300% Modulus 0.00560 GPa
0.812 ksi
Measured on films cast from solution in toluene; ISO 27
Kraton® G1650 E (SEBS) Linear Triblock Copolymer
Description: Kraton G1650 E is a clear linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 29.2% mass. It is supplied from Europe in the physical forms i..
300% Modulus 0.00560 GPa
0.812 ksi
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N774 (SRF) Filler
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..