Polymer Property : 300% Modulus = 0.820 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.00565 GPa
0.820 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 65A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..
300% Modulus 0.00565 GPa
0.820 ksi
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer, Hardness 65A
MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c..