Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.007281 GPa @Time 7200 sec |
1.056 ksi @Time 2.00 hour |
Die C; ASTM D412 |
STAR Thermoplastic Alloys & Rubbers StarXTRUDE XTR-95-1000 TPE Product Description: StarXTRUDE XTR-95-1000 is an easy processing TPE designed for extrusion. Features:Soft TouchRubbery FeelMatte finishExcellent chemical and oil resistanceAdherence to PC, ABS & P.. |