Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00862 GPa | 1.25 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 1-D Heavy Oil Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00860 - 0.0135 GPa | 1.25 - 1.96 ksi | Cure: 40 mins at 135°C; ISO 37 |
Kraton® Cariflex™ IR0307 K Polyisoprene Description: Cariflex IR0307 KU polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its Logarithmic Inherent Viscosity (LIV) va.. |
|||
300% Modulus | 0.00860 - 0.0135 GPa | 1.25 - 1.96 ksi | Cure: 40 mins at 135°C; ISO 37 |
Kraton® IR307 Polyisoprene Description: Kraton IR307 polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its limiting viscosity number of 7.75 dl/g. Regi.. |
|||
300% Modulus | 0.00860 GPa | 1.25 ksi | NBR Conductive Hose Compound |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
300% Modulus | 0.00862 GPa | 1.25 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 1-D Heavy Oil Plasticizer MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00862 GPa | 1.25 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00862 GPa | 1.25 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Hi-Sil 233 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |