Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00931 GPa | 1.35 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 65A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00930 GPa | 1.35 ksi | ASTM D412 |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
300% Modulus | 0.00930 GPa | 1.35 ksi | ASTM D412 |
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
300% Modulus | 0.00931 GPa | 1.35 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber, Hardness 65A MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
300% Modulus | 0.00930 GPa | 1.35 ksi | Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 5565 Dense Extruded Profile FormulationNordel® IP 5565 |
|||
300% Modulus | 0.00931 GPa | 1.35 ksi | Method A (Dumbbell & Section), 20 in/min; ASTM D412 |
PolyOne Synprene® RT-3890M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
300% Modulus | 0.00930 GPa | 1.35 ksi | ISO 37 |
Termopol Termoton® K2GA4055D TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |