Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00940 GPa | 1.36 ksi | DIN 53504 |
Lubrizol ESTANE® T4057 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
300% Modulus | 0.00940 GPa | 1.36 ksi | ASTM D412 |
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |